Not sure what material is best for your application?
Contact an Expert
Tag Archives: chemical etching
Posted on May 2, 2017 by dean
Q: I’m running a semiconductor wet chemical etching process that utilizes 85 % phosphoric acid at around 150-160°C. I need a material that can withstand this process. Super Duplex hex bolts are not cutting it. A: At that particular concentration and temperature high performance nickel alloys like Hastelloy C276 bolts … Continue reading →