Q: Your strength chart for A286 says it offers 120-160 ksi tensile strength. What does this mean? And how can I insure I get bolts that are 160ksi? Is this the spec ASTM A453 Grade 660? A: We can insure you get your bolts made to this tensile strength but … Continue reading →
Posted in Application, FAQs, High Strength, Material, Specialty Metal Fasteners | Tagged A286 bolt per ASTM A453, A286 bolt to 160ksi, A286 cold worked, A286 cold-worked bolt, A286 cold-worked screw, A286 per ASTM A453, A286 screw per ASTM A453, A286 screw to 160ksi, A286 to 160ksi | Leave a comment
Posted on July 7, 2021 by Kathleen
Q: We are currently using A286 bolts per ASTM 453 at 1200F and are having some issues with durability as the tensile strength we originally calculated necessary was 130ksi but seems like we need higher strengths. Any ideas? A: In this type of environment you should consider A-286 in the … Continue reading →
Posted in Application, FAQs, High Strength, High Temperature Resistance, Material, Specialty Metal Fasteners | Tagged A286 ASTM 453 bolt, A286 ASTM 453 bolts, A286 ASTM 453 screw, A286 ASTM 453 screws, A286 bolts compared to Inconel 718 bolts, A286 bolts compared to Inconel bolts, A286 cold-worked bolt, A286 cold-worked bolts, A286 cold-worked screw, A286 cold-worked screws, A286 screws compared to Inconel 718 screws, A286 screws compared to Inconel screws, Inconel 718 bolts compared to A286 bolts, Inconel 718 screws compared to A286 screws, Inconel bolts compared to A286 bolts, Inconel compared to A286, Inconel screws compared to A286 screws | Leave a comment