Tag Archives: Titanium fastener galvanic corrosion
Posted on June 16, 2021 by Kathleen
Q: I’m using metric Grade 5 titanium bolts, washers and nuts for automotive application. Since the car will never be exposed to any salt water environments do I need to worry about galvanic corrosion? A: Galvanic corrosion is really only a problem if you have a liquid medium between the … Continue reading →
Posted in Application, Corrosion Resistance, FAQs, Material, Specialty Metal Fasteners | Tagged Titanium bolt for automotive application, Titanium bolt galvanic corrosion, Titanium bolts for automotive application, Titanium bolts galvanic corrosion, Titanium fastener galvanic corrosion, Titanium fastener or automotive application, Titanium fasteners for automotive application, Titanium fasteners galvanic corrosion, Titanium screw for automotive application, Titanium screw galvanic corrosion, Titanium screws for automotive application, titanium screws galvanic corrosion | Leave a comment