Q: We are installing bolts into a refinery wharf. After doing a test run on a few A316 stainless steel bolts, they came back heavily corroded. Do you have an coating that can be used for salt water applications that would prevent this? Or do can you advise on another … Continue reading →
Posted in Application, Corrosion Resistance, FAQs, Specialty Metal Fasteners | Tagged bolts for saltwater wharf, fasteners for saltwater wharf, Monel 400, Monel 400 bolts for saltwater corrosion resistance, Monel 400 fasteners for saltwater corrosion resistance, Monel bolts for saltwater corrosion, monel bolts for wharf fasteners, monel fasteners for saltwater corrosion, Monel K500 for salt water corrosion resistance, Monel K500 screws for saltwater corrosion resistance, monel screws for saltwater corrosion, screws for saltwater wharf, titanium bolts for saltwater wharf, titanium grade 5 bolts for saltwater corrosion, titanium grade 5 fasteners for saltwater corrosion, titanium grade 5 screws for saltwater corrosion | Leave a comment
Posted on November 15, 2017 by dean
Q: I have a high strength application that requires resistance to damp salt air and occasional sea splash, I’m using Monel 400 but it’s not holding up the the 75ksi of yield I need. Lots of broken bolts? Is is corrosion or strength? Thoughts? A: Your issue isn’t the corrosion. … Continue reading →
Posted on November 14, 2017 by dean
Q: Is AL6XN a steel or nickel alloy? Trying to figure out if it would perform as well as Monel in seawater. A: To answer your first question, AL6XN bolts are actually both a nickel and a steel alloy. AL6XN is often described as a high nickel content stainless alloy. Though … Continue reading →
Posted in Application, Corrosion Resistance, FAQs, Material, Specialty Metal Fasteners | Tagged AL-6XN, AL6XN, Alloy 400, Corrosion, Crevice Corrosion, Monel, Monel 400, pitting, pitting corrosion, salt water, salt water corrosion, sea water corrosion, seawater, stagnant salt water, stagnant water | Leave a comment
Posted on November 2, 2017 by dean
Nickel alloys are a special class of metals containing high levels of nickel (often greater than 20%). They play a key role in industry for their unique combination of high strength, corrosion resistance to harsh acids (like hydrochloric and sulfuric) and high temperature stability. This two-part newsletter will help summarize the distinct benefits of the … Continue reading →
Posted in Application, Blog, Corrosion Resistance, Material, Specialty Metal Fasteners | Tagged AL-6XN, AL6XN, Alloy 20, Alloy 400, Alloy K500, Carpenter 20, Corrosion, corrosion resistance, Monel, Monel 400, Monel K500, nickel, nickel alloys, Salt Water Resistance, Sea Water Resistance, Specialty Metals, Sulfuric Acid | Leave a comment
Posted on July 10, 2017 by dean
Q: I have a salt water environment with high velocities and a lot of debris including sand, dirt and particles. Because of the amount of debris, I’m concerned about what material would work best. A: Both Monel and Titanium can be good choices in this situation. Both perform extremely well … Continue reading →
Posted on May 22, 2017 by dean
Q: I’m using hydrogen fluoride used in a manufacturing process to make refrigerants. I know it’s very corrosive and have tried both hastelloy and inconel fasteners, which I thought were super corrosion resistant. What am I doing wrong because the acid is still eating them? Should I try Tantalum? A: … Continue reading →
Posted in Corrosion Resistance, FAQs, Specialty Metal Fasteners | Tagged aeration, Alloy 400, Fluoride layer, Fluoride passive layer, Hastelloy, HF, Hydrofluoric acid, Monel, Monel 400, oxidizing salts, tantalum | Leave a comment
Posted on May 11, 2017 by dean
They rhyme, are both used in extreme environments, and are both nickel metal alloys, but Monel and Inconel are actually very different. But how? Let’s start with basic chemistry. Monel is a nickel-copper alloy and Inconel is a nickel-chromium alloy. So what does that mean for your extreme application? We … Continue reading →
Posted in Application, Blog, Corrosion Resistance, High Strength, High Temperature Resistance, Specialty Metal Fasteners | Tagged Alloy 400, Alloy 625, Corrosion, hastelloy C2000, High Temperature, Hydrofluoric acid, Inconel, Inconel 625, Monel, Monel 400, saltwater corrosion, sea water corrosion | 1 Comment
Posted on September 21, 2016 by dean
With over 30% of marine equipment failures being the result of marine corrosion, the subsequent costs have added up; now seawater corrosion costs are estimated at 4 % of the GNP. Unfortunately, sea water is not a simple medium because it is chemically and biologically active, which can have an … Continue reading →